Skip to main content
. 2018 Mar 30;10(4):390. doi: 10.3390/polym10040390

Figure 4.

Figure 4

(A) UV/VIS spectrum of hypoxia-responsive mesoporous silica nanoparticles (HR-MSN) incubated under normoxic and hypoxic conditions for 3 h. Measurements were performed in PBS buffer containing 100 μM NADPH as an electron donor. The illustration shows the reduction of nitro to amine under hypoxic conditions; (B) Time-dependent change in surface charge potentials of HR-MSN incubated under normoxic and hypoxic conditions; and, (C) In vitro DOX release profiles from DOX-CD-HR-MSN.