Size (Dh), size distribution (PDI), and Z-potential of 0.1% w/v pristine and thiolated CS-g-PMMA nanoparticles in water at 25 and 37 °C, as measured by DLS.

Copolymer T [°C] Non-crosslinked nanoparticles Crosslinked nanoparticles
Dh (nm) ± S.D. (Relative intensity %) PDI Z-Potential (mV) Dh (nm) ± S.D. (Relative intensity %) PDI Z-Potential (mV)
Unmodified CS-g-PMMA 25 127 ± 9 (100) 0.389 +27 241 ± 11 (100) 0.192 +18
Thiolated CS-g-PMMA 156 ± 6 (94)
25 ± 3 (6)
0.288 +33 221 ± 11 (100) 0.237 +26
Unmodified CS-g-PMMA 37 184 ± 4 (100) 0.201 +25 332 ± 52 (100) 0.336 +17
Thiolated CS-g-PMMA 155 ± 5 (94)
28 ± 1 (6)
0.282 +37 192 ± 5 (100) 0.228 +29