Skip to main content
. 2018 May 17;10(5):538. doi: 10.3390/polym10050538

Figure 6.

Figure 6

Advancing (errors from ±0.52 (PETref) to ±16.31 (Sisal/PET0.10)) and receding (errors from ±2.21 (Sisal/PET0.10) to ±7.53 (Sisal/PET0.13)) contact angles between the water droplet and the surface of the electrospun mats.