Skip to main content
. 2018 May 22;10(5):563. doi: 10.3390/polym10050563

Figure 3.

Figure 3

(a) Frequency shift (absolute value) of four sensors with different PSMA-MIP film thicknesses to 10 ng mL−1 PSMA vs. rebinding time; and (b) reproducibility characterization (different colors represent independent sensor by the same fabrication process).