Figure 5

ATR-FTIR spectra of silicone rubbers exposed to the environments under temperature cycling from −20 °C~90 °C after different cycles, (a) 50 temperature cycles; (b) 100 temperature cycles; (c) 150 temperature cycles; (d) 200 temperature cycles.