Skip to main content
. 2019 Feb 14;12(4):571. doi: 10.3390/ma12040571

Figure 4.

Figure 4

EDS characterisation of the chemical elemental percentages of the evaporant source (0% power), and the SS thin films deposited with a starting beam power of 3% up to 10%. The bars at the top and bottom of each data point indicate the maximum and minimum range of each element percentage of the stainless steel 316L composition and was attained from the XRF device installed database.