. 2017 Nov 14;9(11):615. doi: 10.3390/polym9110615

Figure 10.

Figure 10

(a) FTIR spectra of volatilized pyrolysis products evolved by anaerobic pyrolysis of WPCs at the maximum of mass loss rate; the absorption intensities of the characteristic peaks of (b) hydrocarbons, (c) CO2, and (d) carbonyl compounds.