Skip to main content
. 2017 Aug 26;9(9):394. doi: 10.3390/polym9090394

Figure 2.

Figure 2

Gel Permeation Chromatography (GPC) traces of SG1-terminated PDEAEMA at various reaction times. DEAEMA (0.26 mol, 47.57 mL), styrene (0.03 mol, 3.47 mL), NHS-BlocBuilder® (2.9 mmol, 1.4038 g), SG1 (0.32 mmol, 0.1022 mL). Polymerization was run at 80 °C for 1 h.