Skip to main content
. 2017 Oct 23;9(10):545. doi: 10.3390/polym9100545

Table 1.

The average Ecorr and icorr values determined according to the cathodic and anodic polarization Tafel curves in Figure 3.

Specimens Ecorr (mV) icorr (nA/cm2)
Bare 316L SS −196.2 97.5
2% PCL −129.6 84.7
3% PCL 96.0 0.1
4% PCL 84.9 0.3