Skip to main content
. 2017 Aug 17;9(8):366. doi: 10.3390/polym9080366

Figure 6.

Figure 6

AFM amplitude images (10 × 10 µm2, scale bar = 2 µm) of sheets from different sources. (a) B PF sulfite pulp; (b) B SF sulfite pulp; (c) UB PF kraft pulp; (d) UB SF kraft pulp; (e) MP fines; (f) MFC 1; (g) MFC 2; (h) MFC 3.