Table A2.

Nanocellulose characteristics. All data, except residual fibres, are previously published in [25].

Sample Charge Density (mmol/g) Intrinsic Viscosity (mL/g) Fibril Diameter (nm) Fibril Length (μm) Residual Fibres (%)
Mechanically fibrillated CNF 0.1 620 <100 >1 1.3
Oxidized CNF 0.9 1 450 <20 >1 28.5

1 Aldehyde content was determined for the oxidized quality; 0.2 mmol/g CNF.