Skip to main content
. 2017 Aug 31;9(9):406. doi: 10.3390/polym9090406

Table 1.

Processing conditions for the liquid-assisted extrusion process showing the final material compositions.

Materials Feeding Rate (kg/h) Composition of Materials (wt %)
PLA Suspension PLA TEC ChNC
PLA 2.00 1.56 1 100 - -
PLA-ChNC 1.94 1.56 2 97.0 - 3
PLA-TEC2.5 1.95 1.55 3 97.5 2.5 -
PLA-TEC2.5-ChNC 1.89 1.61 4 94.5 2.5 3
PLA-TEC5.0 1.90 1.60 3 95.0 5.0 -
PLA-TEC5.0-ChNC 1.84 1.66 4 92.0 5.0 3
PLA-TEC7.5 1.85 1.65 3 92.5 7.5 -
PLA-TEC7.5-ChNC 1.79 1.71 4 89.5 7.5 3

1,2,3,4 Fed into extruder, and 1.50 kg/h of water and ethanol were removed as vapor during extrusion. 1 Water and ethanol; 2 Water, ethanol, and ChNC; 3 Water, ethanol, and TEC; 4 Water, ethanol, TEC, and ChNC.