Skip to main content
. 2017 Nov 12;9(11):603. doi: 10.3390/polym9110603

Figure 13.

Figure 13

The bottom surfaces in the mid-span region of the epoxy-based CFRP samples after 6-month water immersion at 20 °C: (a) controlled samples, (b) the unstrained samples, (c) samples under 30% strain level, (d) samples under 58% strain level.