Table showing the bulk resistance and ionic conductivity of the prepared electrolytes.

Electrolyte Rb (ohm) Conductivity (S cm−1)
Liquid 29.74 1.72
E3 30.01 1.61
E4 31.53 1.58
EC1 84.69 0.59
EC2 129.15 0.38
EC3 164.1 0.30