Skip to main content
. 2017 Dec 16;9(12):724. doi: 10.3390/polym9120724

Figure 4.

Figure 4

Calorimetric curves (heating rate: 20 °C/min) of PBS, P(BSmBEPSn) and P(BS70BEPS30) copolymers: (a) 1st scan; (b) 2nd scan after quenching from the melt; and (c) magnification in the Tg region of 2nd scan.