Skip to main content
. 2019 Feb 1;11(2):227. doi: 10.3390/polym11020227

Figure 1.

Figure 1

SEM images of the γ–PGA/β–TCP composite fibrous mats with different γ–PGA/β–TCP weight ratios and different cystamine treatment times: (a) 20:1, 12 h; (b) 20:1, 24 h; (c) 40:1, 12 h; and (d) 40:1, 24 h. (e) The diameter of the electrospun γ–PGA/β–TCP composite fibers (*** p < 0.005). Scale bars: 2 μm.