SEM images of the residues obtained after cone calorimetry for RTM6 samples at 35 kW·m−2 for 500 s with: (a) 35% Actilox; (b) 30% Actilox + 5 % TAHHT-DOPO; (c) 30% Actilox + 5% TAHHT-DDPO surface; (d) 30% Actilox + 5% TAHHT-DDPO inside a hole; (e) 35% Dispersal; (f) 30% Dispersal + 5% TAHHT-DOPO; (g) 30% Dispersal + 5% TAHHT-DDPO.