Table 4.
Interlaminar shear strength (ILSS) of selected carbon fiber-reinforced thermoset polymers (CFRP) samples additionally normalized to RTM6 + CF.
Sample | ILS (N·mm−2) | Relative ILSS (%) |
---|---|---|
RTM6 + CF | 67.8 ± 3.2 | 100 ± 5 |
+ 10% BA-DOPO | 65.4 ± 2.0 | 97 ± 3 |
+ 10% TAHHT-DOPO | 67.4 ± 1.8 | 99 ± 3 |
+ 10% TAHHT-DDPO | 71.0 ± 2.3 | 105 ± 4 |