Mean diameter, standard deviation and smallest measured diameter of at least 30 carbon fibers in composite materials with partially flame retarded RTM6 after irradiation at 60 kW·m−2 for 20 min determined by SEM.

Sample Mean Diameter (µm) Smallest Diameter (µm)
RTM6 + CF 3.3 ± 0.7 2.1
+ 10% BA-DOPO 5.2 ± 0.3 4.7
+ 10% TAHHT-DOPO 5.3 ± 0.2 4.9
+ 10% TAHHT-DDPO 6.3 ± 0.4 5.3
+ 10% TAHHT-DOPO-DDPO 5.9 ± 0.3 5.3