Skip to main content
. 2019 Feb 20;11(2):368. doi: 10.3390/polym11020368

Table 1.

The different samples with different reaction parameters.

Projects Parameters
Addition of methylcellulose 0, 30 wt %, 50 wt %, 70 wt %, and 100 wt %
STMP concentration 0.1 wt %, 0.2 wt %, 0.3 wt %, 0.4 wt %, and 0.5 wt %
Crosslinking time 0.5 h, 1.5 h, 2.5 h, 3.5 h, and 4.5 h