Skip to main content
. 2019 Feb 21;11(2):380. doi: 10.3390/polym11020380

Table 4.

X-ray photoelectron spectroscopy (XPS) results of the residual char of EP and EP/polysulfone composites.

Sample C (% a) N (%) O (%) P (%) S (%)
EP 82.82 3.22 13.77 0.10 0.09
EP/ArPN2 Inner 82.49 1.10 16.10 0.13 0.18
EP/ArPN2 Outer 79.19 3.16 16.65 0.84 0.17
EP/ArPO2 Inner 81.80 1.11 16.74 0.14 0.21
EP/ArPO2 Outer 75.52 2.88 19.28 2.05 0.26
EP/ArOPN2 Inner 80.87 1.09 17.52 0.28 0.24
EP/ArOPN2 Outer 71.34 5.53 19.78 2.92 0.43
EP/ArOPO2 Inner 80.92 3.26 14.35 1.24 0.23
EP/ArOPO2 Outer 72.17 4.50 19.98 2.87 0.48

a Atomic concentration.