Table 5.
WVTR as well as the swelling of LDPE as well as the prepared WPC containing different concentration of modified and unmodified lignocellulosic fibers.
| Samples | Lignocellulosic fibers, % | WVTR, g/(m2. Day) | Thickness swelling, % |
|---|---|---|---|
| LDPE | 0.0 | 0.005 | 0.20 |
| WPC5C | 5.0 | 1.711 | 0.72 |
| WPC10C | 10.0 | 48.322 | 0.87 |
| WPC20C | 20.0 | 61.302 | 1.20 |
| WPC5F | 5.0 | 10.204 | 0.69 |
| WPC10F | 10.0 | 12.343 | 0.75 |
| WPC20F | 20.0 | 20.818 | 0.95 |