Figure 6.
4-point bending strength (a), area under the stress-displacement curves (b) and selected stress-displacement curves (c) of cured laminates from oil-based CPC paste and 3 layers of SES PCL scaffolds with and without treatment in 1.0 or 2.0 M NaOH. Exemplarily, reproducibility regarding the preparation regime was analyzed with respect to laminate thickness, maximal bending force, bending strength and area under the force-displacement curves was analyzed using laminates of oil-based CPC paste and 3 layers of SES PCL scaffolds treated with 2.0 M NaOH for 30 min (d).