Skip to main content
. 2019 Feb 26;12(5):687. doi: 10.3390/ma12050687

Figure 4.

Figure 4

SEM images of the top and bottom parts of porous α-SiAlON samples fired under different conditions: 1800 °C-2 h (A1, A2), 1900 °C-1 h (B1, B2) and 1900 °C-2 h (C1, C2).