Fig. 4.

Fig. 4

Microstructure analysis of as-prepared and tensile-deformed copolymers. a, b Two-dimensional (2D) wide-angle X-ray diffraction (WAXD) patterns of P4 and ultra-strong elastomer 4 (uE4); c WAXD azimuthal intensity profiles for P4 and uE4 at 2θ = 21°; d a proposed model to illustrate the microstructure rearrangement of P(UDA-co-BUDA) copolymers during cyclic tensile deformation