Figure 2.

Figure 2

Plots of log[−ln(1 − X(t))] vs. logt of the representative samples isothermally crystallized at the predetermined temperatures: (a) PLA/TPEE (80/20); (b) PLA/TPEE/ADR (80/20/0.5); (c) PLA/TPEE/ADR (80/20/1.0).