. 2016 Dec 8;8(12):417. doi: 10.3390/polym8120417

Figure 9.

Figure 9

SEM micrographs of PLA/TPEE/ADR samples annealed at 80 °C for 40 min: (a) PLA/TPEE (80/20); (b) PLA/TPEE/ADR (80/20/0.5); (c) PLA/TPEE/ADR (80/20/1.0).