Skip to main content
. 2016 Oct 11;8(10):357. doi: 10.3390/polym8100357

Figure 8.

Figure 8

TTI and PHRR values of 171 g/m2 PET fabrics treated with 5, 10, and 20 BL of silica/silica nanoparticles deposited by dipping (A) [25]. Comparison between same LbL architectures deposited by dipping and spray on 490 g/m2 PET (B) [26]. Data obtained by cone calorimetry at 35 kW/m2.