Combustion data of untreated and NP-treated PET-COT_65:35 by cone calorimetry (35 kW/m2) [22].

Sample TTI ± σ [s] THR ± σ [MJ/m2] PHRR ± σ [kW/m2] FPI ± σ [s·m2/kW] [CO] yield ± σ [Kg/Kg] [CO2] yield ± σ [Kg/Kg]
PET-COT_65:35 (245 g/m2) 11 ± 1 3.4 ± 0.2 140 ± 5 0.08 ± 0.06 0.0313 ± 0.0021 2.91 ± 0.03
PET-COT_65:35_CNa 24 ± 4 3.7 ± 0.1 125 ± 7 0.19 ± 0.13 0.0328 ± 0.0049 2.54 ± 0.11
PET-COT_65:35_SiO2 20 ± 1 3.6 ± 0.1 130 ± 5 0.15 ± 0.04 0.0265 ± 0.0028 2.57 ± 0.21
PET-COT_65:35_HT 74 ± 1 2.7 ± 0.3 121 ± 1 0.61 ± 0.01 0.0304 ± 0.0023 2.71 ± 0.54
PET-COT_65:35_HTSiO2 54 ± 1 2.6 ± 0.3 115 ± 4 0.47 ± 0.03 0.0281 ± 0.0041 2.69 ± 0.47