. 2016 Oct 11;8(10):357. doi: 10.3390/polym8100357

Table 8.

Combustion data of untreated and LbL-treated PET by flame spread tests according to the ASTM D6413 standard [25].

Sample Burning time [s] Afterflame time [s] Dripping Weight loss [%]
PET (171 g/m2) 32 20 YES 8
5 BL 10 - NO 1
10 BL 2 - NO -
20 BL 10 - YES 2