Skip to main content
. 2016 May 26;8(6):205. doi: 10.3390/polym8060205

Table 1.

Pore radius of the untreated, thermostabilised and carbonised lignin samples. Errors of the respective fit and calculations, respectively, are given in brackets.

Sample Name n P/Q (m2·cm−3) R/(nm)
untreated −3.85(5) 97(20) -
thermostabilised −3.87(2) 130(30) -
carbonised −3.45(2) 770(50) 1.06(4)