Skip to main content
. 2016 Apr 7;8(4):124. doi: 10.3390/polym8040124

Figure 5.

Figure 5

Delamination and longitudinal cracking on a fretting fatigue tested strap. Strap tested for N = 9 × 104 cycles at 800 MPa.