Skip to main content
. 2016 Jun 22;8(6):242. doi: 10.3390/polym8060242

Figure 9.

Figure 9

Dynamic mechanical analysis (DMA) charts for dry CFRP sample; (a) before moisture saturation and after; (b) the first (120 °C, 72 h); (c) third moisture saturation cycles. The red line indicates the position that noises are appeared due to the delamination of CF layers.