Details of the experimental program.

Environmental Type FRP Type Loading Level Exposure Duration/Times Number of Specimens
Freeze–thaw cycles CFRP 0, 30%, 60% 0, 50, 100, 200, 300 times 90
GFRP 0, 30% 60
Hygrothermal aging CFRP 0, 30%, 60% 0, 30, 90, 180, 360 days 90
GFRP 0, 30% 60
Wet–dry cycles CFRP 0, 30%, 60% 0, 30, 90, 180, 360 times 90
GFRP 0, 30% 60