Skip to main content
. 2017 Apr 7;9(4):133. doi: 10.3390/polym9040133

Figure 3.

Figure 3

X-ray diffraction patterns (CuKα) of: graphene oxide (eGO, with O/C, wt/wt = 0.62); CB sample with the highest BET specific surface area; this CB after oxidation (oCB-3, O/C, wt/wt = 0.91). Patterns in the 2θ range 4–40° (A) and enlarged patterns in the 2θ range 40–85° (B).