Table 1.

Water contact angle measurements of PU/PLDL blend cast films doped with different amounts of zinc oxide.

Sample Water contact angle (°)
PU/PLDL (control) 81.3 ± 0.9
PU/PLDL 0.05 ZnO 95.7 ± 4.5
PU/PLDL 0.01 ZnO 101.3 ± 5.8
PU/PLDL 0.001 ZnO 115.7 ± 6.3