POM images of (a1a4) 70/30, (b1b4) 50/50 and (c1c4) 30/70 PVDF/PCL blends. The blend samples were first cooled from 190 to 150 °C for the crystallization of PVDF and then quenched to 30 °C to crystallize PCL.