Skip to main content
. 2016 Sep 20;8(9):316. doi: 10.3390/polym8090316

Figure 6.

Figure 6

XRD patterns of the cellulose/HA nanocomposites prepared by microwave-assisted hydrothermal method at 180 °C for 10 min using different phosphorus sources: (a) NaH2PO4·2H2O; (b) ATP; (c) CP; (d) FBP.