Skip to main content
. 2016 Aug 26;2:16037. doi: 10.1038/micronano.2016.37

Figure 15.

Figure 15

Thermoluminescence glow curves of four sets of Al2O3:C particles exposed before irradiation to PETN detonations, compared with a pristine control. All glow curves were stimulated using a linear heating ramp of ~0.9 °C s−1 (Ref. 27).