Skip to main content
. 2016 Aug 26;2:16037. doi: 10.1038/micronano.2016.37

Figure 3.

Figure 3

Thermoluminescent intensity versus temperature (‘glow curve’) for an Mg2SiO4 particle after being subjected by microheater to ~190 ms heating pulses of varying maximum temperatures. (An SEM of a similar particle and microheater can be seen in Figure 11.) Note the two peaks, each corresponding to a different class of trap34.