The amount of PEDOT:PSS that was transferred from glass to PDMS with different diffusion times was counted by testing the conductivity of PEDOT:PSS/PEG on the PDMS substrate. The normalized diffusion length was converted from normalized conductivity, which was directly proportional to the thickness of the PEDOT:PSS film. The red dashed line represents the relationship between the normalized diffusion length and saturated diffusion time; it also separates the graph into two regions, where region 1 is time-dependent and region 2 is thickness-dependent.