Skip to main content
. 2019 Apr 2;8(4):418–428. doi: 10.1002/open.201900004

Table 3.

Table showing the ESR of each of the graphene membranes before and after 10,000 GCD cycles measured using EIS.

Material

Before Cycling

After Cycling

ESR / Ω

ESR/Ω

GO

2.5±0.2

1.6±0.2

rGO

1.1±0.1

7.2±0.6

LEG

0.9±0.1

0.9±0.1

CEEG

0.3±0.1

0.3±0.1

AEEG

0.7±0.1

0.5±0.1

GNR

0.6±0.1

0.4±0.1