Fig. 8.

Fig. 8

(A) XRD pattern of untreated and treated Ti with 2 kW PP and scanning speed of 0.2 mm s−1, (B) XRD pattern of; β-TCP coat, titanium substrate and ICDD standard β-TCP 55-0898.