Skip to main content
. 2019 Apr 2;7:183. doi: 10.3389/fchem.2019.00183

Figure 7.

Figure 7

Evolution of the layer thickness and mass deposited per pulse for different tOFF durations and a fixed 1ms tON (error bars: means ± SD, n = 3).