EIS parameter of DSSC employed with different TBP concentration.

Sample Rs(ohm-cm2) RCT(ohm-cm2) RTiO2(ohm-cm2)
0.1 M Li-+ + 0.5 M TBP 12 6,960 57,697
0.1 M Li-+ + 0.8 M TBP 44 1,275 17,652