Table 2.
Physical properties of different catalyst carriers.
| Sample | BET surface area/(m2·g−1) | Pore volume/(cm3·g−1) | Average pore diameter/nm |
|---|---|---|---|
| TiO2-CA | 78.3 | 0.378 | 15.10 |
| TiO2-SA | 79.9 | 0.339 | 14.29 |
| TiO2-500 | 129.7 | 0.344 | 8.61 |
| TiO2-600 | 55.3 | 0.308 | 17.52 |
| Ti-Ce-Ox-500 | 144.3 | 0.358 | 8.23 |
| Ti-Ce-Ox-600 | 77.9 | 0.337 | 14.39 |