N2 adsorption measurements for CATT, CPER and CLAY samples at different firing temperatures.

Sample Specific Surface Area (m2/g) Total Pore Volume (cm3/g) Pore Diameter (nm)
CLAY 800 °C 18.3 0.12 5.46
CLAY 1000 °C 7.02 0.05 1.84
CATT 800 °C 29.53 0.16 2.36
CATT 1000 °C 11.94 0.09 1.61
CPER 800 °C 19.1 0.13 3.66
CPER 1000 °C 9.24 0.08 2.42