Skip to main content
. 2019 Mar 16;12(6):887. doi: 10.3390/ma12060887

Table 2.

Description of raw materials used in polyurethane synthesis.

Compound Supplier Short Description Structure Formula
PCL diol
(CapaTM 2200)
Perstrop,
Malmo, Sweden
Linear polyestrodiol, terminated with hydroxyl groups; Appearance: white, waxy solid; Average molecular weight: 2000 g/mol; Melting temp: 40–50 °C;
Density: 1.05 g/cm3; Viscosity at 60 °C: 480 mPa s;
Purity> 99%.
graphic file with name materials-12-00887-i001.jpg
HDI Sigma-
-Aldrich,
Taufkirchen, Germany
Aliphatic diisocyanate; Appearance: colorless liquid;
Molar mass = 168.2 g/mol; Boiling point: 255 °C; Melting point: −67 °C; Density (25 °C) = 1.05 g/cm3; Purity> 99%;
LD50 (rat) = 746 mg/kg.
graphic file with name materials-12-00887-i002.jpg
BDO Brenntag,
Essen, Germany
Low molecular weight chain extender Molar mass =
90.12 g/mol; Appearance: colorless liquid; Purity> 95.5%;
Melting point: 20.4 °C; Density (20 °C) = 1.02 g/cm3
graphic file with name materials-12-00887-i003.jpg