Ti6Al4V deposited along a linear trajectory during two passes of the laser beam and powder nozzle: (a) 800 W peak power and 0.3 m/min scanning speed; (b) 1000 W peak power and 0.3 m/min scanning speed; (c) 1200 W peak power and 0.3 m/min scanning speed; (d) 1200 W peak power and 1 m/min scanning speed. Magnification bar: 1 mm.