Skip to main content
. 2019 Mar 19;12(6):906. doi: 10.3390/ma12060906

Figure 16.

Figure 16

(a) MTS results for the SaOs2 cells grown on Laser Melting Deposition (LMD) printed Ti6Al4V; (b) SEM micrograph of SaOs2 cells 3 days after seeding on LMD printed Ti6Al4V; Fluorescence microscopy images of SaOs2 cells cultivated for (c) 1 day and (d) 3 days on the surface of LMD printed Ti6Al4V.